What was found
DURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE AROUND SCREW HOLES ON THE LT FILLET SKIN BETWEEN STA 1120-1146 L26L TO L29L, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AND PRIMED AREA IAW DC-8 SRM 51-1-8. BLENDED CORROSION IAW DC-8 SRM 51-1-8, 53-2-0 FIG 1F AND 51-1-21.