What was found
DURING A MAINTENANCE VISIT, FOUND CORROSION DAMAGE TO PANEL P AT STA 420, X-55 TO -60, Z0. DAMAGE EXCEEDED LIMITS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED NEW SECTION AND SPLICE PLATES IAW DC8 SRM 53-2-3 FIG 9 AND 51-3-0. (CORROSION DAMAGE RECORDED IN EWA CORROSION PROGRAM).