ABI - STRINGER 19L WAS FOUND TO BE CHAFFED BEYOND SRM LIMITS AT SKIN JUNCTION 05. BLENDED CHAFED AREA. PERFORMED AN EDDY CURRENT INSPECTION OF THE BLENDED AREA. NO DEFECTS NOTED. FABRICATED A DOUBLER ANGLE, TWO SHIMS. REPAIR DONE IAW EMB 145 SRM (145/1142, CHAPTER 53, REV 20) 53-24-02 AND STANDARD SRM PRACTICES. (M)