What was found
DURING AN MBV INSPECTION OF THE FUSELAGE A DENT AFT OF FRAME 363 ON THE LEFT SIDE, WAS FOUND TO BE BEYOND SRM LIMITS. COMPLETELY REMOVED THE DAMAGED BY CREATING A 2.7 INCH BY 1.1 INCH CUTOUT. PERFORMED AN EDDY CURRENT INSPECTION OF THE CUTOUT. NO DEFECTS NOTED. FABRICATED A REPAIR DOUBLER. REPAIR DONE IAW SAAB 340 SRM, 72LKS 3079 REV 43, 53-70-10 PARA 4 FIG 209 AND STANDARD SRM PRACTICES. (M)