What was found
SSI 53-23-005 RH BEAM BETWEEN CROSSBEAMS FR90-91 IS CORRODED (LEVEL 2 CORROSION)-C/A-REMOVED AND REPLACED ANGLE BRACKET ON R/H BEAM BETWEEN CROSSBEAMS FR90-91IAW EMB 170 SRM 51-40-08
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
SSI 53-23-005 RH BEAM BETWEEN CROSSBEAMS FR90-91 IS CORRODED (LEVEL 2 CORROSION)-C/A-REMOVED AND REPLACED ANGLE BRACKET ON R/H BEAM BETWEEN CROSSBEAMS FR90-91IAW EMB 170 SRM 51-40-08