What was found
FWD SIDE OF BS 663 VAPOR BARRIER RH SIDE UPPER ATTACH ANGLE UPPER END CRACKED BS663; RBL8; WL167. / [01] UPDATED MEASUREMENT TABLE; [02] CONFORMED -1 REPLACEMENT ANGLE AND -2 SPLICE ANGLE PER SRM 57-10-10-2R-5 THE -1 REPLACEMENT ANGLE FABRICATED IN ACCORDANCE WITH SRM 57-10-10-2R REPAIR 5 REFER TO ATS BUILD RECORD ATSHFAB-101-354 JOB # 539510 THE -2 SPLICE ANGLE FABRICATED IN ACCORDANCE WITH SRM57-10-10-2R-5 REFER TO ATS BUILD RECORD ATSHFAB-101-355 JOB # 539866; [03] CONFORMED -1 REPLACEMENT ANGLE AND -2 SPLICE ANGLE PER SRM 57-10-10-2R-5 THE -1 REPLACEMENT ANGLE FABRICATED IN ACCORDANCE WITH SRM 57-10-10-2R-5 REFER TO ATS BUILD RECORD ATSHFAB-101-354 JOB # 539510 THE -2 SPLICE ANGLE FABRICATED IN ACCORDANCE WITH SRM 57-10-10-2R-5 REFER TO ATS BUILD RECORD ATSHFAB-101-355 JOB # 539866; [04] REMOVED DAMAGED AREA AND PREPARED REPAIR AREA FOR INSPECTION BS 663 RBL6-14 WL 167 IAW SRM 57-10-10-2R-5.; [05] VERIFIED REMOVED DAMAGED AREA AND PREPARED REPAIR AREA FOR INSPECTION BS 663 RBL6-14 WL 167 IAW SRM 57-10-10-2R-5.;