What was found
CORROSION AFT CARGO BAY ON FLOOR PANEL SPLICE BS887 RBL 10 TO LBL 6 WL 156 ; / [01] CORROSION ON SPLICE WAS FOUND TO BE OUT OF LIMITS DUE TO NO LIMITS ARE GIVEN IN THE SRM. SPLICE WILL BE REMOVED AND REPLACED PER SRM 51-10-02-0G-0 PARAGRAPH 9.; [02] INSPECTED AND VERIFIED CORROSION ON SPLICE WAS FOUND TO BE OUT OF LIMITS DUE TO NO LIMITS ARE GIVEN IN THE SRM. SPLICE WILL BE REMOVED AND REPLACED PER SRM 51-10-02-0G-0 PARAGRAPH 9.; [03] REMOVED AFT CARGO BAY FLOOR PANEL SPLICE BS887 IAW SRM 51-40-02-0G-0; [04] OK TO INSTALL AFT CARGO BAY FLOOR PANEL SPLICE BS887 GIVEN; [05] INSTALLED AFT CARGO BAY FLOOR PANEL SPLICE BS887 IAW SRM 51-40-02-0G-0;DWG#146A7500; [06] VERIFIED CORRECTIVE ACTION ENTRY 5. CARD COMPLETE