What was found
LT HORZ STAB LOWER SKIN CRACKED RIB STA 194 APPROX. 9.5 INCHES FROM FRONT SPAR ; / [01] CUT OUT DAMAGE IAW SRM 55-10-01-2R-11.; [02] VERIFIED DAMAGE CUTOUT PER NDT PART 6 51-00-00 PROCEDURE 23 AND SRM 55-10-00-2R-11.; [03] FABRICATED REPAIR DOUBLER IAW SRM 55-10-01-2R-11; [04] C/W; [05] FABRICATED REPAIR PARTS IAW SRM 55-10-01-2R-11.; [06] FABRICATED REPAIR PARTS IAW SRM 55-10-01-2R-11. C/W INSPECTION; [07] OK TO INSTALL REPAIR PARTS.; [08] OK TO INSTALL REPAIR PARTS.<BR>RII INSPECTION C/W.; [09] INSTALLED REPAIR PARTS IAW SRM 55-10-01-2R-11.; [10] INSTALLED REPAIR PARTS IAW SRM 55-10-01-2R-11.<BR>RII INSPECTION C/W.; [11] OK TO INSTALL 331 BZ.; [12] REPAIRED SKIN CRACK IAW SRM 55-10-01-2R-11.