What was found
RT HORZ. LOWER SKIN HAS CRACK AT RIB STA 194 APPROX 16.5 INCHES FROM FRONT SPAR APPROX .75 LONG ; / [01] CUT AND REMOVED DAMAGE I.A.W SRM 55-10-01-2R-11.; [02] VERIFIED DAMAGE CUTOUT CORRECTIVE ACTION 1 PER NDT PART 6 51-00-00 PROCEDURE 23 AND SRM 55-10-00-2R-11.; [03] FABRICATED REPAIR DOUBLER I.A.W SRM 55-10-01-2R-11.; [04] FABRICATED REPAIR PARTS IAW SRM 55-10-01-2R-11. C/W INSPECTION; [05] INSTALLED REPAIR PARTS PER SRM 55-10-01-2R-11.; [06] COMPLIED WITH INSPECTION OF STEP 5; INSTALLATION OF REPAIR PARTS. INSTALLATION OK.; [07] REPAIRED LOWER SKIN CRACK PER SRM 55-10-01-2R-11; [08] INSPECTED WORK PERFORMED