What was found
CORROSION FOUND AFT CARGO DOOR LOWER SILL STRAP FROM STA 787 TO STA 847 HAS SPOTS OF CORROSION. ; / [01] REMOVED CORROSION AT AFT CARGO DOOR LOWER SILL STRAP FROM STA 787 TO STA 847 AS PER REF B737-700 SRM 51-10-02-0G-0; [02] VERIFIED STEP # 1.; [03] PERFORMED UT THICKNESS INSP ON REWORKED AREA AFT CARGO COMPT IAW B737 NDT P4 51-00-00 PROC.3; MIN THK. NOTED 0.071'<BR>TOOL USED : OLYMPUS 27MG B/C 172139 04/22; [04] ORIGINAL THICKNESS .100'; MATERIAL REMOVED 0.029'; MATERIAL REMAINING 0.071'. FOUND OUT OF LIMITS AS PER SRM 53-60-15-1A-1; [05] VERIFIED STEP # 4.; [06] REMOVED AFT CARGO DOOR SILL STRAP FROM STA 787 TO STA 847<BR>AS PER REF B737-700 SRM 51-40-02-0G-0; [07] LOCATED AND DRILL NEW STRAP AS PER REF B737-700 SRM 51-40-05-0G-0; [08] VERIFIED STEP NO 7. LOCATED AND DRILL NEW STRAP AS PER REF B737-700 SRM 51-40-05-0G-0; [09] OK TO INSTALL STRAP.; [10] INSTALLED AFT CARGO DOOR LOWER SILL STRAP FROM STA 787 TO STA 847 AS PER REF B737-700 SRM 51-10-02-0G-0 AND DWG 146A8128; [11] REMOVED CORROSION AT AFT CARGO DOOR LOWER SILL STRAP FROM STA 787 TO STA 847. FOUND OUT OF LIMITS; REPLACED STRAP AS PER REF B737-700 SRM 51-10-02-0G-0 AND DWG 146A8128; [12] VERIFIED STEPS 10 AND 11.