What was found
ACD SUB THRESHOLD CORRODED AT BS 794, 794+8, BS807+13 &+17, RBL 26. REMOVED LIGHT SURFACE CORROSION AT ACD SUB THRESHOLD IAW SRM 51-60-15-0I-1. UT THICKNESS TESTED BLENDED AREA IAW NDT PART 451-00-00 PROCEDURE 2. EVALUATED DAMAGE ON THRESHOLD WEB MORE CORROSION WAS FOUND. REMOVED CORROSION ON THRESHOLD WEB IAW SRM51-10-02-0G-0 FOUND TO BE OUT OF LIMITS. REWORKED AREA IAW SRM 53-00-53-1A-2, ALLOWABLE DAMAGE PARAG. 4.A (2) DETAIL (E) FIG 103. LOCATED AND DRILLED NEW SUB THRESHOLD IAW SRM 51-40-05-0G-0. INSTALLED ON CARD TTG8Q004E31T.