What was found
SUPPLEMENTAL INFORMATION: IN THE FORWARD CARGO AREA ON THE RIGHT HAND SIDE PLATE; THERE IS EVIDENCE OF CORROSION AT STATION 500A+6. ; / [01] FOUND TO BE OUT OF LIMITS PER SRM 53-00-53-1A-2; [02] TOOL INFO ONLY.; [03] REMOVED AND REPLACED TRANSITION ANGLE AT RBL 21.8 FORM STA 500 TO 500D PER SRM 51-40-02.; [04] INSPECTION C/W REPLACEMENT OF TRANSITION ANGLE FROM STA 500 THRU STA 500D RBL 21.8 PER SRM 51-40-02