What was found
SUPPLEMENTAL INFORMATION: ABOVE L1 CUTOUT LWR END OF FRAME BS 312 APPEARS TO BE CRACKED AT RADIUS BETWEEN S-5L AND S-6L. 8-95 ; / [01] REMOVED EXISTING FASTENERS FOR ACCESS TO REPAIR IN IAW SRM 51-40-02-0G-0; [19] INSTALLED REPAIR ANGLE AT L-1 CUTOUT LWR OF FRAME BS 312 BETWEEN S-5L AND S-6L IN IAW SRM 53-10-07-2R-1 FIG 202 AND 203 SHEET 1; [20] APPLIED A LAYER OF BMS 3-23; TYPE LL CORROSION INHIBITING COMPOUND ON THE SURFACE OF REPAIR AREA IN IAW AMM 51-21-91-620-801; [21] FABRICATED AND INSTALLED REPAIR ANGLE AT L-1 CUTOUT LWR OF FRAME BS 312 BETWEEN S-5L AND S-6L IN IAW SRM 53-10-07-2R-1 FIG 202 AND 203 SHEET 1; [22] VERIFIED STEPS 18;19;20 AND 21.