FWD CARGO COMP.RH SIDEWALL ANGLE STA 500D CORRODED ABOVE Z-ANGLE / BLENDED OUT CORROSION FROM STA 500D SIDEWALL RAIL ANGEL IAW SRM 53-00-53-1A-2. STEP 2D. MAT LOSS 0.014'. ORIGINAL THICKNESS 0.071' THE MATERIAL REMAINING 0.057'. THE AREA FOUND TO BE OUT OF LIMIT IAW SRM 53-00-53-1A-2 FIGURE 103 LOCATED AND DRILLED NEW RAIL ANGEL P/N 143A9485Y34 IAW SRM