What was found
47D) FASTENER AND SKIN DAMAGED AT STA 247. 2IN. ABOVE L/H NLG W/W. / CHEMICALLY REMOVED PAINT AND INSPECTED DAMAGE WITH 10X MAGNIFIER. REPAIRED DAMAGE PER SRM 53-00-01-2R-41 AND 53-00-01-1A-1 SURFACE BLENDING. DAMAGE DIMENSIONS LENGTH 0.040??? X WIDTH 0.040??? X DEPTH 0.003???. ACCOMPLISHED HOLE PROBE INSPECTION OF FASTENER HOLES PER NDT PART 6 ; 51-00-00 PROCEDURE 16 AND COUNTERSINK INSPECTION PER NDT PART 6 ;53-30-00 PROCEDURE 3. NO DEFECTS NOTED. FASTENER LOCATION AND FINISH RESTORATION ENCOMPASSED IN REPAIR DOUBLER REFERENCE EA 1-753-32077.