What was found
B.S. 663 VAPOR BARRIER UPPER ATTACH ANGLE IS CRACKED AT R.B.L. 12; W.L. 164. / [01] VERIFIED APPLICABILITY OF SRM 57-10-10-2R-5 TO BE CORRECT AND UPDATED MEASUREMENT TABLE;[07] RECEIVED REPAIR PARTS FROM OSS FOR BS 663 VAPOR BARRIER UPPER ATTACH ANGLE RBL 12 WL 164; REPLACEMENT ANGLE RO# 863967-SWA; AND SPLICE ANGLE RO# 863969-SWA.;[08] VERIFIED ACTION 7;[09] LOCATED AND DRILLED NEW ATTACH ANGLE AND SPLICE ANGLE PER SRM 51-40-05-0G-0 AND SRM 57-10-10-2R-5;[10] APPLIED CHEMICAL CONVERSION COATING AND PRIMER ON REPAIR PARTS PER SRM 57-10-10-2R-5 REPAIR 5;[11] LOCATED AND DRILLED NEW ATTACH ANGLE AND SPLICE ANGLE PER SRM 51-40-05-0G-0 AND SRM 57-10-10-2R-5 REPAIR 5;[12] VERIFIED CORRECTIVE ACTION ITEM 9-11; OK TO INSTALL PER SRM 57-10-10-2R-5.;[13] INTERNAL CAP SEAL OF REPAIR FASTENERS INSIDE OF FUEL CELL BS 663 RBL 5-22 WL 164 IS DOCUMENTED ON CARD TTG8Q00BSMHH.;[14] INSTALLED REPAIR PARTS ON BS 663 VAPOR BARRIER UPPER ATTACH ANGLE RBL 12 WL 164 PER SRM 57-10-10-2R-5 REPAIR 5;