What was found
#8 SLAT O/B LOWER SURFACE OF THE WEDGE IS CRUSHED AND DELAM. / [01] DELAMINATION TO LOWER SURFACE OF #8 SLAT IS OUT OF LIMITS IAW SRM 57-42-01-1A-1;[02] ACCOMPLISHED PRE #8 SLAT INSTALLATION BORESCOPE INSPECTION. NO DEFECT NOTED.;[03] OK TO INSTALL #8 SLAT.;[04] ACCOMPLISHED POST SLAT CAN BORESCOPE INSPECTION. NO DEFECT NOTED.;[05] R&R #8 SLAT PER M/M 27-81-21.;[06] C/W INSPECTION.;[07] SEE INDIVIDUAL SIGN OFFS FOR RII INSPECTION.