What was found
CORROSION ON R/H TRANSITION ANGLE UPPER SURFACE AROUND NUT PLATE HOLES BS 500A TO BS 500D. / [01] REMOVED DAMAGE I.A.W SRM 51-10-02. MEASURED DAMAGE DEPTH TO BE .008 INCHES. DAMAGE FOUND TO BE BEYOND ALLOWABLE DAMAGE LIMITS AS GIVEN IN SRM 53-00-53-1A-2.;[09] FABRICATED AND INSTALLED RH TRANSITION ANGLE AND REPAIR SPLICE FROM STA 500A TO STA 500D+10 PER SRM 53-00-53;SRM 51-40-02; AND EA 22-153-01343. REFER TO EACH STEPS FOR WORK ACCOMPLISHED.;