What was found
LH HORIZONTAL STAB; LWR STAB SKIN CRACKED AT STAB STA 193.90; CUTOUT LOWER HORIZONTAL SKIN OF L/H HORIZONTAL STAB PER SRM 55-10-01-2R-11 STEP 4 (B) 2. AND DRILLED OUT EXISTING FASTENERS IN REPAIR AREA PER STEP 4 (F) 1. FABRICATED REPAIR DOUBLER PER SRM 55-10-01-2R-11 STEP4 G; DOUBLER FABRICATED FROM LOT #1468128-1 2024-T3; FILLER FABRICATED FROM LOT #1468136-12024-T3. FILLER FABRICATION;APPLIED CHEMICAL CONVERSION AND PRIMER PER SRM 55-10-01-2R-11 STEP 4 (M) AND (N);INSTALLED REPAIR DOUBLER IAW SRM 55-10-01-2R-11 REPAIR 11.TOTAL SURFACE AREA FOR REPAIR DOUBLER IS 78.375 SQUARE INCHES IAW SRM 55-10-01-2R-11 REPAIR 11 STEP 1 H APPLIED SEALANT AROUND EDGES OF DOUBLER IAW SRM 55-10-01-2R-11 REPAIR 11 STEP 4Q;