What was found
CRACK ON LOWER L/H COMPOSITE BULKHEAD I/B UPPER ATTACH ANGLE AT LBL 7 BS 663. / [01] VERIFIED APPLICABILITY IAW SRM 57-10-10-2R-5;[02] REMOVED 8 EA FASTENERS COMMON TO FUEL TANK AND CUT OUT DAMAGE ANGLE IAW IAW SRM 57-10-10-2R-5;[03] VERIFIED CORRECTIVE ACTION #2;[04] HFEC INSPECTED TRIMMED EDGE OF DAMAGE CUTOUT AND OPEN FASTENER HOLES IN REPAIR AREA PER 737NDT PART 6 51-00-00 PROCEDURES 23 AND 16. NO CRACKS FOUND. TOOL N500 IS000450 DUE 02/2023;[05] RECEIVED NEW FILLER REPAIR P/N:ATSHFAB-101-353 LOT:547726 AND SPLICE REPAIR P/N:ATSHFAB-101-355 ; LOT:54[17] INSTALLED FASTENERS ON UPPER ATTACH ANGLE COMMON TO VAPOR BARRIER; BS 663 IAW SRM 51-40-02-0G-0; SRM 57-10-10-2R-5; AND DWG 111A1000;