What was found
AFT CARGO BAY FLOOR SPLICE HAS CORROSION AROUND NET PLATE HOLE BS887 LBL6.5 WL167.5 / [01] UPDATED MEASUREMENT TABLE FOR PICTURE OF CORROSION ATTACHED;[02] CORROSION ON SPLICE FOUND TO BE OUT OF LIMITS DUE TO NO LIMITS ARE GIVEN IN THE SRM.;[03] VERIFIED CORRECTIVE ACTIONS 1 AND 2<BR><BR>VERIFIED MEASUREMENTS TABLE<BR><BR>VERIFIED PICTURE OF CORROSION IS ATTACHED;[04] REMOVED AND REPLACED AFT CARGO BAY FLOOR STRAP AT BS 887 WL 167.5 PER SRM 51-40-02-0G-0 AND DWG 146A7500;[05] VERIFIED CORRECTIVE ACTION 4.