What was found
CRACK AROUND THE FASTENER AT THE NR 7 SLAT LOWER SURFACE, AT ACTUATOR RIBS. REMOVED FASTENERS IAW SRM 51-40-02. HFEC INSPECTED OPEN HOLES IAW NDTM PART 6 51-00-00, PROCEDURE 16. CONFIRMED CRACKS WITHIN INSPECTION AREA. HFEC INSPECTED COUNTERSINKS IAW NDTM PART 6 53-30-00, PROCEDURE 3. CONFIRMED CRACKS IN COUNTERSINKS. TRIMMED OUT THE DAMAGE IAW SRM 57-42-01-2R-8. FABRICATED REPAIR DOUBLER, FILLER, APPLIED CHEMICAL CONVERSION COATING IAW SRM 57-42-01-2R-8 FIG 202 ALTERNATIVE 1, & PRIMED. INSTALLED THE REPAIR IAW SRM 57-42-01-2R-8, FIG 202, ALTERNATIVE 1.