What was found
CRACKED STRINGER AT AREA AFT OF FCB BS535 S-23L WL164. MARKED<REMOVED DAMAGED SECTION OF S-23L BETWEEN BS 500D TO 540 RECEIVED STRINGER SECTION FROM OSS R.O # 913318-SWA IAW SRM 53-00-03-2R-1 REP.1 PAR.D;[08] VERIFIED CORRECTIVE ACTION STEP 7.;[09] RECEIVED STRINGER SPLICE HAT CHANNEL FROM OSS R.O # 913318-SWA IAW SRM 53-00-03-2R-1 REP.1 PAR.D;[10] VERIFIED CORRECTIVE ACTION #9;[11] LOCATED; DRILLED AND APPLIED CHEMICAL CONVERSION COATING ON REPAIR PARTS AND REPAIR AREA OF S-23L AND BETWEEN BS 500D TO 540 IAW SRM 53-00-03-2R-1 REP.1 PAR.D TO I.;[12] VERIFIED CORRECTIVE ACTION 11. OK TO PRIME GIVEN;[13] APPLIED PRIMER ON REPAIR PARTS AND REPAIR AREA OF S-23L AND BETWEEN BS 500D TO 540 IAW SRM 53-00-03-2R-1 REP.1 PAR J. AND OK TO INSTALL OF REPAIR PARTS AND REMOVED PARTS FOR REPAIR;[14] VERIFIED CORRECTIVE ACTION ITEM 13.<BR>OKAY TO INSTALL REPAIR PARTS AND PARTS REMOVED TO FACILITATE REPAIR GIVEN.;[15] INSTALLED ALL REPAIR PARTS S-23L AND BETWEEN BS 500D TO 540 IAW SRM 53-00-03-2R-1 REP.1 PAR. K; EA 23-153-01115; DWG. 143A3210 AND 143A1215.;[16] UPDATED STEPS 1 AND 2.THE DAMAGE WAS REPAIRED PER 737-700 SRM 53-00-03-2R-1 (REPAIR 1) AND EA 23-153-01115.