What was found
LEFT VAPOR BARRIER UPPER ANGLE CRACKED AT FASTENER HOLE LBL 2' CORRECTION ON ORIGINAL WRITE UP LEFT VAPOR BARRIER UPPER ANGLE CRACKED AT FASTENER HOLE LBL 6'<[01] OK TO APPLY ALODINE AND PRIMER COAT TO REPAIR PARTS.;[02] TREATED WITH ALODINE AND PRIMER REPAIR PARTS AS PER 737-700 SRM 51-20-01-0G-0 AND 51-21-72-370-804;[03] VERIFIED ALODINE AND PRIMER APPLICATION.;[04] OK TO INSTALL REPAIR PARTS; FILLER AND ANGLE.;[05] OK TO APPLY CUP SEAL TO FASTENER HEADS.;[06] REPAIRED DAMAGE AT VAPOR BARRIER UPPER ATTACH ANGLE STA 663 LBL 6 AS PER B 737-700 SRM 57-10-10-2R-5 FIG 202 DETAIL B SHEET 4;[07] VERFIED WORK ACCOMPLISHED AND DOCUMENTATION;[08] RII. VERIFIED WORK STEPS PROCESS.;[09] VERIFIED COMPLETE WORK PERFORMED