What was found
INTERNAL - HORIZONTAL PRESSURE DECK WEB STA 663 TO STA 675 - CRACK NOTED IN INSPECTION AREA RBL 39 TO RBL 60. MARKED LOCATION.<[01] VERIFY APPLICABILITY FOR THE BEADED PRESSURE DECK WEB REPAIR BETWEEN STA 663.75 AND STA 675 RBL 38 TO RBL 60 B737-700 SRM 53-40-51-2R-2 REPAIR 2 EFFECTIVITY: ALL;[02] REMOVED DAMAGE FROM BEADED PRESSURE DECK WEB BETWEEN STA 663.75 AND STA 675 RBL40 TO RBL60 PER B737-700 SRM 53-40-51-2R-2 REPAIR 2[16] INSTALLED NEW REPAIR PARTS FOR BEADED PRESSURE DECK WEB STA 663 TO STA 675 RBL60.00 TO RBL30 PER B737-700 SRM 53-40-51-2R-2 REPAIR 2. REQUIRE CAPSEAL SOME FASTENERS.;[17] VERIFIED CORRECTIVE ACTION 16 INSTALLATION;[18] CAPSEAL FASTENERS AND CIC REPAIR AREA PER B737-700 51-30-01 AND AMM 51-00-59/201.;[19] CAPSEALED FASTENERS AND CIC REPAIR AREA PER B737-700 AMM 51-31-00-390-805 AND AMM 51-00-59/201.;[20] VERIFIED CORRECTIVE ACTION STEPS 18 AND 19.;[21] UPDATED MEASUMENT TABLE... JOB COMPLETED;[22] VERIFIED CORRECTIVE ACTION 21; VERIFIED MEASUREMENT TABLE.