What was found
AFT CARGO COMPARTMENT LEFT TRANSITION ANGLE HAS SURFACE CORROSION BETWEEN STA 727J-747.<[01] EDITED THE FAULT FROM AFT CARGO COMPARTMENT RIGHT TRANSITION ANGLE HAS SURFACE CORROSION BETWEEN STA 727J-747. [TTG8Q00KLY4M] TO AFT CARGO COMPARTMENT LEFT TRANSITION ANGLE HAS SURFACE CORROSION BETWEEN STA 727J-747. [TTG8Q00KLY4M] PER INSPECTION SUPERVISOR LARRY FLIPPO REQUEST.;[02] REMOVED SURFACE CORROSION ON L/H TRANSITION ANGLE AT STA. 727J-747 PER SRM 51-10-02. REMOVED .008? OF MATERIAL. MATERIAL REMAINING THICKNESS IS .032' AND FOUND TO BE OUT OF LIMITS PER SRM 53-00-53-1A2;[03] C/W INSPECTION;[04] FAULT RESOLVED ON TTG8Q00KRJY6;[05] FAULT RESOLVED ON TTG8Q00KRJY6