What was found
BS 663 LH SIDE VAPOR BARRIER WEB HAS CRACKS AND A TEMPORARY REPAIR; LBL 6 TO LBL 15.<[01] IDENTIFIED IAW SRM 57-10-10-0I-2 FIGURE 2 TABLE 2 ITEM 4<BR><BR>DAMAGE EXCEEDS ALLOWABLE DAMAGE LIMITS IAW SRM 57-10-10-1A-2 PAR.4 D(1)<BR><BR>DAMAGE TO BE REPAIRED IAW SRM 51-70-04-2R-10 AS DIRECTED BY SRM 57-10-10-2R-2 PAR.1 C(NOTE)<BR><BR>REMOVED DAMAGED PLIES MEASURING 6'X4'; CLEANED; WITH NO CONTAMINATION NOTED IAW SRM 51-70-04-2R-10 PAR.4 A-C;[02] VALIDATED REPAIR PER SRM 51-70-04-2R-10;[03] VERIFIED CORRECTIVE ACTIONS 1 AND 2<BR><BR>VERIFIED MEASUREMENTS TABLE<BR><BR>VALIDATED REPAIR PER SRM 51-70-04-2R-10;[04] FABRICATED REPAIR PLIES FROM BMS9-3 ST1581 LOT#1526805-2 IAW SRM 51-70-04-2R-10 PAR.4 D<BR><BR>OK TO INSTALL