What was found
AFT CARGO TRANSITION ANGLE RBL 22' STA.727J TO STA.747. HAS AREAS OF CORROSION AROUND FASTENER HOLES.<[01] REMOVED LIGHT SURFACE CORROSION AFT CARGO R/H TRANSITION ANGLE FROM STA. 727H-727I PER SRM 51-10-02; FOUND TO BE OUT OF LIMITS. MATERIAL REMOVED .007 AND REMAINING THICKNESS .033 PER SRM 53-00-53-1A-2.;[02] CORRECTION ON LINE 1. REMOVED LIGHT SURFACE CORROSION AFT CARGO R/H TRANSITION ANGLE FROM STA. 727J-747 PER SRM 51-10-02; FOUND TO BE OUT OF LIMITS. MATERIAL REMOVED .007 AND REMAINING THICKNESS .033 PER SRM 53-00-53-1A-2.;[03] FOR COMPANY CONVENIENCE R/H TRANSITION ANGLE TO BE REPAIR ON NON-ROUTINE TTG8Q00M0H7M FROM STA. 727+4 TO 767.;[04] VERIFIED C/A # 2 (TECHNICIAN); 06-JUL-2023 10:01 UTC<BR>CORRECTION ON LINE 1. REMOVED LIGHT SURFACE CORROSION AFT CARGO R/H TRANSITION ANGLE FROM STA. 727J-747 PER SRM 51-10-02; FOUND TO BE OUT OF LIMITS. MATERIAL REMOVED .007 AND REMAINING THICKNESS .033 PER SRM 53-00-53-1A-2.;[05] VERIFIED C/A # 3 (TECHNICIAN); 06-JUL-2023 22:56 UTC<BR>FOR COMPANY CONVENIENCE R/H TRANSITION ANGLE TO BE REPAIR ON NON-ROUTINE TTG8Q00M0H7M FROM STA. 727+4 TO 767.;[06] CW