What was found
FWD GALLEY DOOR CUTOUT LOWER 'L' ANGLE ATTACHED TO Z ANGLE HAS CORROSION 5EA FASTENER HOLES.(MARKED)<[01] REMOVED CORROSION IAW SRM 51-10-02. DAMAGE REMOVAL APPROX .015' OUT OF LIMITS PER SRM 53-10-15-1A-2.;[02] LOCATED/DRILLED FASTENER HOLES IN REPLACEMENT ANGLE AND INSTALLED 5 EACH NUT PLATES IAW SRM 51-10-02 AND SRM 51-40-02.;[03] INSPECTED WORK ACCOMPLISHED IN C/AA #'S 1 AND 2.<BR><BR>1. JASON BORN (TECHNICIAN); 06-JUL-2023 13:48 UTC REMOVED CORROSION IAW SRM 51-10-02. DAMAGE REMOVAL APPROX .015' OUT OF LIMITS PER SRM 53-10-15-1A-2.<BR><BR>2. JASON BORN (TECHNICIAN); 07-JUL-2023 12:37 UTC LOCATED/DRILLED FASTENER HOLES IN REPLACEMENT ANGLE AND INSTALLED 5 EACH NUT PLATES IAW SRM 51-10-02 AND SRM 51-40-02.;[04] R/R 'L' ANGLE IAW SRM 51-40-02.;[05] INSPECTED WORK ACCOMPLISHED.