What was found
FWD CARGO RH TRANSITION ANGLE HAS CORROSION FROM STA. 500E TO 500F.<[01] BLENDED AREAS; REMOVED .010' MATERIAL; FOUND TO BE OUT OF LIMITS PER SRM 53-00-53-1A-2.;[02] REMOVED DAMAGE FROM STA. 500D+10 TO 500F+10 PER SRM 53-00-53-2R-5. FABRICATED REPAIR PARTS PER SRM 53-00-53-2R-5 AND EA EA M-22-153-01550.;[03] RII INSPECTED AS REQUIRED. CORRECTIVE ACTION #1 AND #2;[04] RII OK TO INSTALL REPAIR PARTS.;[05] REMOVED DAMAGE FROM STA. 500D+10 TO 500F+10 PER SRM 53-00-53-2R-5. FABRICATED REPAIR PARTS PER SRM 53-00-53-2R-5 AND EA EA M-22-153-01550. INSTALLED REPAIR PARTS PER SRM 53-00-53-2R-5 AND EA M-22-153-01550.;[06] C/W INSPECTION.;[07] REMOVED DAMAGE FROM STA. 500D+10 TO 500F+10 PER SRM 53-00-53-2R-5. FABRICATED REPAIR PARTS PER SRM 53-00-53-2R-5 AND EA EA M-22-153-01550. INSTALLED REPAIR PARTS PER SRM 53-00-53-2R-5 AND EA M-22-153-01550.;[08] RII; COMPLIED WITH INSPECTION; REMOVED DAMAGE FROM STA. 500D+10 TO 500F+10 PER SRM 53-00-53-2R-5. FABRICATED REPAIR PARTS PER SRM 53-00-53-2R-5 AND EA EA M-22-153-01550. INSTALLED REPAIR PARTS PER SRM 53-00-53-2R-5 AND EA M-22-153-01550.