What was found
CORROSION ON FLOOR BEAM AT STA 947.5 AND RBL 24.75 LAV HARD POINT<[01] REMOVED CORROSION AT STA 947 RBL 24; ORIGINAL THICKNESS .180' REMOVED .045' REMAINING MATERIAL THICKNESS .135' REF B737 SRM 53-70-51-1A-1 REMOVED AND REINSTALLED LAV HARDPOINT AT STA 947.5 RBL 24.75 REF BAC DWG 147A5650 AND B737NG SRM 51-40-02 ALL OTHER REPAIR WORK ACCOMPLISHED ON CUSTOMER CARD TTG8Q00S2B45 AND HAECO CARD 42283.;[02] VERIFIED REMOVED CORROSION AT STA 947 RBL 24; ORIGINAL THICKNESS .180' REMOVED .045' REMAINING MATERIAL THICKNESS .135' REF B737 SRM 53-70-51-1A-1 REMOVED AND REINSTALLED LAV HARDPOINT AT STA 947.5 RBL 24.75 REF BAC DWG 147A5650 AND B737NG SRM 51-40-02 ALL OTHER REPAIR WORK ACCOMPLISHED ON CUSTOMER CARD TTG8Q00S2B45 AND HAECO CARD 42283.