What was found
FWD CARGO R/H TRANSITION ANGLE UPPER SURFACE HAS CORROSION AT N/P AND FASTNER HOLES STA 500H - 500I RBL 23-25 WL 156. MRKD<[01] REMOVED CORROSION PER SRM 51-40-02. BLENDED AREA OUT OF LIMITS PER SRM 53-00-53-1A-2.;[02] WRONG REFERENCE WAS USED FOR DAMAGE REMOVAL. <BR>REMOVED CORROSION PER SRM 51-10-02. BLENDED AREA OUT OF LIMITS PER SRM 53-00-53-1A-2;[03] INSPECTED/ VERIFIED THE WORK PERFORMED ON CORRECTIVE ACTION ON #2; NO DEFECTS NOTED.;[04] REFERENCE FAULT TTG8Q00SVS21: R/H TRANSITION ANGLE P/N 143A7501-188 STA 500A TO STA 500I REPLACED PER SRM 51-40-02.;[05] CORRECTION MADE TO MEASUREMENT #1.;[06] VERIFIED CORRECTIVE ACTION #4