What was found
CORROSION ON AFT CARGO COMPARTMENT LH SIDE PLATE BETWEEN STA 747-767 (MARKED)<[01] REMOVED CORROSION FROM AFT CARGO LEFT SIDE PLATE FROM STA 747-767 ORIGINAL MATERIAL THICKNESS IS 0.040?; MAX MATERIAL LOSS IS 0.005; MAX ALLOWED IS 0.004 ?; FOUND TO BE OUT OF LIMITS PER SRM 53-00-53-1A-2;[02] TOOL T010008 S/N 503011WAS NOT USED;[03] SEE WORK CAPTURE # TTG8Q00UALJZ FOR REPLACEMENT OF LH SIDE PLATE;[04] INSPECTED WORK ABOVE