What was found
(CUSTOMER REQUEST) CRACK ON VAPOR BARRIER LOC. BS 663 BETWEEN RBL 43 TO RBL 50 AT MAIN WHELL WELL 2025-139022<[01] TOOL USED: SCALE PN: CR5200 SN: 8343110875 DUE DATE: 28-FEB-25.;[02] TOOL USED: HOT BONDER P/N: HCS9200B S/N: 18185847 DUE DATE: 01-OCT-25.;[03] TOOL USED: SCALE PN: 91847 SN: AE-409313 DUE DATE:29-JUN-25.;[04] EQUIPMENT P/N EPOCH 600; S/N 130547106; DUE DATE 30-SEP-25 WAS USED ON STEP 12;[05] REPAIRED VAPOR BARRIER LOC. BS 663 BETWEEN RBL 43 TO RBL 50 AT MAIN WHELL WELL IAW B737-800 SRM 51-70-04-2R-10 REPAIR 10. SEE INDIVIDUAL SIGNOFFS BELOW;[06] REPAIRED VAPOR BARRIER LOC. BS 663 BETWEEN RBL 43 TO RBL 50 AT MAIN WHELL WELL IAW B737-800 SRM 51-70-04-2R-10 REPAIR 10. SEE INDIVIDUAL SIGNOFFS BELOW. RII COMPLETED