What was found
FORWARD CARGO LEFT Z-ANGLE HAS MULTIPLE AREAS OF CORROSION AROUND NUT PLATE HOLES FROM BS 500+10 - 500D. REMOVED CORROSION FROM LT ZEE ANFLE BS 500+10 - 500D. EVALUATED REWORKED AREA WITH ORIGINAL THICKNESS 0.040'; LOSS 0.020'; REMAINING .020'. MAXIMUM LOSS OF 0.10T, FOUND TO BE OUT OF LIMITS IAW SRM 53-00-53-1A-2. FABICATED REPLACEMENT SECTION AND REPAIRED IAW SRM 53-00-53-2R-5 AND SRM 51-40-02-0G-0 FROM BS 480+10 - 520.