What was found
DELAMINATION ON TAIL CONE AT 4 O'CLOCK. REMOVED DAMAGED SKIN IAW SRM.53-80-70-2R-1, REPAIR 1, 51-70-05-2R-11, REPAIR 11, SRM 51-70-05-2R-1, REPAIR 1. APPLIED POTTING & CURED IAW SRM.51-70-05-2R-11, REPAIR 11. APPLIED HOT BOND REPAIR TAP TEST FAILED IAW SRM.53-80-70-2R-1, REPAIR 1, 51-70-05-2R-11, REPAIR 11, SRM 51-70-05-2R-1, REPAIR 1. REMOVED DELAMINATED REPAIR, & CORE IAW SRM.53-80-70-2R-1, REPAIR 1, 51-70-05-2R-11, REPAIR 11, SRM 51-70-05-2R-1, REPAIR 1. POTTED CORE INSTALLATION IAW SRM 51-70-2R-0, REPAIR GENERAL. PERFORMED WET LAY UP REPAIR IAW SRM 53-80-70-2R-1, REPAIR 1, SRM 51-70-04-2R-3, REPAIR 3, & CURE TO SRM 51-70-04-2R-0, REPAIR GENERAL.