What was found
DURING CHECK-C MAINT, THE RT WING NUMBER 7 LE SLAT HAD A REPAIR 3.5 INCH BY 2.75 INCH THAT WAS DELAMINATED ON INBD SIDE. INSTALLED A 3.5 INCH BY 2.75 INCH HOT BOND REPAIR PER SRM 51-70-10.