What was found
DURING CHECK-C MAINT, FOUND DELAMINATION ON LT WING UPPER LE 2.5 FEET BEHIND NR 6 LE SLAT, OTBD END, 5 INCHES LONG. REPAIRED SURFACE WITH A 3 IN BY 5 IN HOT BOND REPAIR PER SRM 51-70-08, PG 6 THRU 32.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
DURING CHECK-C MAINT, FOUND DELAMINATION ON LT WING UPPER LE 2.5 FEET BEHIND NR 6 LE SLAT, OTBD END, 5 INCHES LONG. REPAIRED SURFACE WITH A 3 IN BY 5 IN HOT BOND REPAIR PER SRM 51-70-08, PG 6 THRU 32.