What was found
DURING ROUTINE C-CHECK, DISCOVERED DENTS/GOUGES ON THE LOWER SKIN PANEL AT MULTIPLE LOCATIONS, BETWEEN STRINGERS 5 AND 12, AND BETWEEN WS 250 AND WS 720. DAMAGED AREAS WERE BLENDED OUT. THE MAXIMUM BLEND DEPTH WAS 0.016" WHICH IS AT THE AREA COMMON TO STRINGER 5, AT APPROX WS 250. THE BLENDED AREAS AND EFFECTED FASTENER HOLES WERE HFEC INSPECTED. ROTO PEENED AND REFINISHED IAW THE SRM. REPAIRED IAW SRM 51-00-06.