What was found
INSPECTION TYPE-C, RT WING ANTI-ICE TELESCOPIC DUCT, L/E CUT OUT AREA SUSPECT CRACK AT IB AND OB SIDE AS MARKED. HFEC INSP CARRIED OUT IAW DAC NDT SPM R.13,06-10-01.001 & FOUND CRACK AS MARKED. FASTENERS AT CRACKED AREA REMOVED IAW SRM57-31-01V.2 & SRM 57-33-01 V.2R.40. CRACKED AREA TRIMMED OUT IAW SRM 57-10-00 FIG.43V.1R.40. REP DOUBLER & FILLER FAB IAW SRM 57-10-00 FIG.43 V.1R.40. REP DOUBLER HEAT TREAT TO T62 IAW DPS 7.00-1, HARDNESS 83.83 FOUND WITHIN LIMIT IAW DPS 1.05.