LOWER AFT BULK PIT FLOOR HAS HOLE BEYOND AMM LIMITS. INSPECTED FLOOR PANEL FOUND TO BE OUT OF LIMITS PER SRM 53-10-20 FIG 109 SHEET 1. REPLACED FLOOR PANEL PER MM 53-10-20.