What was found
CLT - FOUND KEELBEAM ANGLE CORRODED .750 INCH BY 64 INCHES, LOWER KEEL BEAM LEFT ANGLE STATION 663 TO 727. CORROSION LEVEL 1. REMOVED CORROSION PER SRM 51-10-1. (M)
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
CLT - FOUND KEELBEAM ANGLE CORRODED .750 INCH BY 64 INCHES, LOWER KEEL BEAM LEFT ANGLE STATION 663 TO 727. CORROSION LEVEL 1. REMOVED CORROSION PER SRM 51-10-1. (M)