What was found
THREE EACH RADIATING CRACKS AT STA 480L, BETWEEN S8L & S9L. CUT OUT CRACKED AREA, INSTALLED REPAIR ANGLES PER TR 53-10-20E, DEFECT SIZE: .080 INCH.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
THREE EACH RADIATING CRACKS AT STA 480L, BETWEEN S8L & S9L. CUT OUT CRACKED AREA, INSTALLED REPAIR ANGLES PER TR 53-10-20E, DEFECT SIZE: .080 INCH.