What was found
INT - DURING Q-4 CHECK VISUAL INSPECTION, FOUND CORROSION ON BULKHEAD SUPPORT ANGLE 3 INCH BY 1.5 INCH BS 1016 BULKHEAD (FORWARD FACE) JUST ABOVE DRAIN HOLE BBL '0'0. INSTALLED CHANNEL REPAIR AND SKIN REPAIR, REPAIRED PER SRM 51-40-3 FIG 1 AND SRM 53-10-4 FIG 3. CORROSION TASK NR C53-208-01, CORROSION LEVEL 2. (M)