What was found
CLT - DURING Q-1 CHECK VISUAL INSPECTION FOUND 3 AREAS OF CORROSION 2 INCH BY 4 INCH AT STATION 294.5, RBL 54 Z ANGLE. CORROSION LEVEL 2. INSTALLED NEW Z-ANGLE PER SRM 51-10-2. (M)
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
CLT - DURING Q-1 CHECK VISUAL INSPECTION FOUND 3 AREAS OF CORROSION 2 INCH BY 4 INCH AT STATION 294.5, RBL 54 Z ANGLE. CORROSION LEVEL 2. INSTALLED NEW Z-ANGLE PER SRM 51-10-2. (M)