What was found
DURING EVALUATION OF CORROSION OF FS 280 CIRCUMFERENTIAL JOINT FROM STR 25L TO 25R, STR 27 WAS FOUND TO BE CRACKED AT FASTENER HOLE, 2ND HOLE AFT FROM FS 280 JOINT.
As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.
DURING EVALUATION OF CORROSION OF FS 280 CIRCUMFERENTIAL JOINT FROM STR 25L TO 25R, STR 27 WAS FOUND TO BE CRACKED AT FASTENER HOLE, 2ND HOLE AFT FROM FS 280 JOINT.