What was found
FWD CARGO PIT BILGE AREA; DRAIN PAN SUPPORT ANGLE LOWER SURFACE AND NUT PLATES HAVE CORROSION ABOVE FRAME AT FS 959, S49-51L. REMOVED CORROSION IAW SRM 51-21-01; VOL II; PG 28. THE ORIGINAL THICKNESS IS .040 IAW DWG ADA0145 REV J; THE MATERIAL REMOVED IS .002; MATERIAL REMAINING IS .038. FOUND TO BE WITHIN LIMITS IAW SRM 53-00-01; VOL II; FIG 1B. TREAT AND PRIMED IAW SRM 53-21-01; VOL II; PGS 21 AND 24; THEN INSTALLED NUT PLATES IAW SRM 51-33-01; VOL II; PG 2.