Service difficulty report · Skin · Cndair CL6002B19

Difficulty date
August 20, 2007
Submitted
August 29, 2007
Operation
Air carrier
Aircraft
N467AW
Make and model
Cndair CL6002B19
Aircraft serial
7900
Part
Skin
Condition
Damaged
Location
Rt Wing
Stage of operation
IN
How discovered
9
Nature of condition
O
Precautionary procedure
K

As reported to the FAA. Reports are unverified, and codes are left as the FAA publishes them.

What was found

RIGHT WING LOWER PLANK FUEL TANK ACCESS DOOR CUTOUT AT WS 54.897 9640BB, HOLE NR 1) HAS FRETTING DAMAGE AT INBOARD AND OUTBOARD ENDS OF CUTOUT IN NON-CRITICAL AREA. INBOARD AREA MEASURES APPROX 6 INCH LENGTH BY .30 INCH WIDE BY .005 INCH DEEP. OUTBOARD AREA MEASURE APPROX 5.5 INCH LONG BY .30 INCH WIDE BY .005 INCH DEEP. OUTBOARD AREA MEASURE APPROX 5.5 INCHES LONG BY .30 INCHES WIDE BY .005 INCHES DEEP. MAINTENANCE REPAIRED CORRODED (FRETTING) DAMAGE AREAS IAW REO 601R-57-21-030 REV F. (M)