What was found
AFT CARGO COMPARTMENT FLOOR SUPPORT ANGLE CORRODED AT SPLICE LWR SURFACE AT STA 1445, RBL 3. REMOVED AND REPLACED IAW SRM 51-40-02 REV 98. CORROSION REMOVED SRM 51-10-02 REV 98. ORIGINAL THICKNESS 0.071", MATERIAL REMOVED 0.020", MATERIAL REMAINED 0.051" FOUND EXCEED LIMIT SRM 53-00-53 FIG. 101 REV. 98. THIS REPAIR IS CLASSIFIED AS MINOR IAW GMM 6-2-100 CRITERIA.