What was found
RADIOGRAPHY INSPECTION CARRIED OUT ON TRANSVERSE SKIN SPLICE AT STATION 6-100 AND FOUND 01 EACH CRACK INDICATION AT FORWARD SIDE OF STRINGER 7 LEFT CENTER SPLICE, PROPAGATE FROM SECOND FASTENER FROM CENTER APPROXIMATELY 0.5 INCHES LENGTH. MAIN DECK CARGO STATION 6-100 STRINGER 7 LEFT CRACKED SPLICE FITTING REMOVED AND REPLACED AS PER SRM 51-33-01-OG. SPLICE FITTING FABRICATED BY MACHINING AS PER DOUGLAS DRAWING A6A7112 REVISION A. REPAIR CLASSIFIED AS MAJOR PER GMM 6-2-100.